The general specifications of aluminum alloy lines can be used in a range of 1-3cm in width, 0.5cm-2cm in depth and 0.1-0.25cm in thickness.
02 Line installation Install aluminum alloy line along the ink bucket line (adhesive free).
Thick spraying and full spraying shall be conducted for the first layer, but sagging is not allowed.
Elastic glue line Elastic glue line is the most widely used deep groove line at present.
Plastic separation strips are divided into many types according to the area of use.
In the past two years, the deep groove modeling process of the exterior wall has created a grooving wind in the exterior wall coating market – that is, the marble paint has the effect of dry hanging marble, which is an integral whole.
05 Flushing, polishing and maintenance: polish the putty powder to improve the overall flatness; Flushing maintenance can improve the strength and adhesion of putty (more than 2 times).
It is light in material, simple in technology, and cheap in price.
The roller coating must be in place during construction without missing coating.
(After it is completely dry, use 800 # sandpaper for micro polishing, and the burning surface will be better.) 09 After colorful and dry covering construction, finish oil construction shall be carried out.
01 division (snapping the ink bucket line) In the construction area, pop up the division size with the ink bucket, and pay attention to the determination of the horizontal line.
Thank you for your understanding…
Spraying shall be adopted.
The composite mortar can be scraped in batches again, and the construction can be carried out in combination with the crack resistant fiber grid cloth.
After the cement mortar coarse sand is scraped, the process construction shall be carried out.
The specific area depends on the construction wall area.
04 Exterior wall putty powder construction When mixing putty powder, there must be a maturing process to fully hydrate the putty powder.
Protect the aluminum alloy groove with the same width of textured paper to facilitate the later construction.
Pay attention to the evenness control, no missing coating or hanging, and avoid the generation of yin and yang surfaces, which may cause inconsistent glossiness.
5D groove process advantages 1: strong stereoscopic effect 5D groove process advantages 2: good flatness 5D groove process advantages 3: high fidelity 5D groove process advantages 4: popular and beautiful stone like paint deep groove construction steps: construction tools 1.
The surface oil shall be sprayed or roller coated.
The second construction is carried out by thin spraying.
Under normal circumstances, the line with a width of 1.5-2cm and a depth of 0.7-1cm is the best.
The material is mainly plastic, low cost, light and easy to construct, and the lines are not easy to deform.
Statement: Part of the articles and materials in this public account are from the network, which are only for learning and exchange, and have no intention of infringement.
The following is part of the display of separator strips: 2.
07 During the construction of intermediate coating, roller coating or spraying shall be adopted, and no water shall be added.
Then, the second surface oil construction will be carried out.
06 Sealer Sealer can be roller coated with 30% water to increase its penetration function.
3.
It is no longer distinguished by striking black lines.
Pay attention to the air pressure control of the spray gun.
If you are offended, please contact us to delete them.
08 Stone like color dots shall be prepared in place before construction (air pump requirements, spray gun commissioning).
It is widely used.
Aluminum alloy lines are made of materials with high hardness and thick thickness, and are not easy to deform.
The overall effect is stronger, the style is elegant and unique, and it is loved by the owners! Today, Xiao Bian specially discussed the process of deep groove of marble paint on the exterior wall.
It has a variety of widths and thicknesses, and can adapt to the wall in the corner area.
03 Cement mortar leveling&batch scraping of composite mortar First batch scraping of fine sand cement slurry, the thickness of each batch scraping shall not exceed 0.3cm.
Before construction, ensure that the putty is completely dry, and add water to the sealing primer to adjust the viscosity of the paint; Spraying or roller coating shall be applied once, and the coating shall be even and free of coating leakage and accumulation; Dry for at least 6 hours after construction, and then roll coat the second layer.
For the construction of the first primer, the roller coating is required to be uniform and in place without hanging or missing.